Table 1 Details of the nanofiber formulations and viscosity of electrospinning solutions

From: Fabrication and characterization of tretinoin-loaded nanofiber for topical skin delivery

FormulationComposition %w/vViscosity
PCLTretinoinViscosityTorque
A100.5122.081.8%
B101123.182.4%