Fig. 1From: A multi-targeting bionanomatrix coating to reduce capsular contracture development on silicone implantsSurface images of 30 and 60 layers of bionanomatrix coated silicone implants mimicking contact shear stress conditions after implantation in the breast by SEM analysis. A-F 30 layers of bionanomatrix coating under 0, 30–100 Pa, and 300–500 Pa ranges of contact shear stress. G-L 60 layers of bionanomatrix coating under 0, 30–100 Pa, and 300–500 Pa ranges of contact shear stress. NO-30: 30 layers of bionanomatrix coated silicone, NO-60: 60 layers of bionanomatrix coated siliconeBack to article page