Fig. 9From: Optimization of the clinically approved Mg-Zn alloy system through the addition of Caa Tensile test results of the investigated alloys. b relationship between yield strength and grain size. Tensile test results after immersion in Hank’s solution for 30 days of (c) 0.1% Ca and (d) 0.3% Ca alloysBack to article page