Table 4 Summary of mechanical properties of electrospun tubular scaffolds

From: Effect of sequential electrospinning and co-electrospinning on morphological and fluid mechanical wall properties of polycaprolactone and bovine gelatin scaffolds, for potential use in small diameter vascular grafts

  Yield strain (%) Tensile strength (MPa)
Untreated
B0 44.59 ± 13.78 5.09 ± 0.56
C0 44.88 ± 0.088 8.37 ± 0.12
B1 38.72 ± 3.23 3.46 ± 0.088
C1 37.37 ± 3.72 2.20 ± 0.22
Treated
B0 46.91 ± 13.97 4.60 ± 0.84
C0 43.80 ± 1.45 7.08 ± 0.35
B1 29.54 ± 9.88 2.28 ± 0.006
C1 33.55 ± 4.88 2.87 ± 0.31