Scaffold name | B0 | C0 | B1 | C1 | ||||
---|---|---|---|---|---|---|---|---|
Polymer | PCL | Gelatin | PCL | Gelatin | PCL | Gelatin | PCL | Gelatin |
Technique | sequential electrospinning | co-electrospinning | ||||||
Flow (mL/h) | 1.2 | 0.3 | 0.8 | 0.3 | 1.2 | 0.3 | 0.8 | 0.3 |
Voltage (kV) | 18 | 15 | 18 | 15 | 18 | 15 | 18 | 15 |
Needle-rod gap (cm) | 18 | 15 | 18 | 15 | 18 | 15 | 18 | 15 |
Rod diameter (cm) | 0.6 | |||||||
Rod rotation speed (rpm) | 20 | |||||||
Humidity (%) | 40-50 | |||||||
Temperature (°C) | 28-30 |