From: Increased pore size of scaffolds improves coating efficiency with sulfated hyaluronan and mineralization capacity of osteoblasts

Fig. 2

Characterization of LoPo and HiPo scaffold formulations. Using micro-computed tomography, a the mean porosity, b mean pore size, and c amount of scaffold pores per pore size of LoPo and HiPo (low and high porosity, respectively) scaffolds was analyzed. d The stability of scaffolds was evaluated by compression testing. e Cross and f longitudinal section are presented as well as (g) 3D visualization and (h) REM images of the scaffolds (scale bars: E: 1100 μm, F: 1050 μm, G: 1.500 μm, H: 250 μm). Data represent the mean ± SD. Statistical analysis was performed by student’s t-test. ***: p < 0.001