Table 1 Porosity (%) of PEEK/CS specimens after heat treatment and during ageing (n = 10)

From: Characterisation of a novel poly (ether ether ketone)/calcium sulphate composite for bone augmentation

Ageing time (Days)

PEEK content (%)

0

2.5

20

40

80

0

70.7 ± 3.15

72.1 ± 0.49

73.9 ± 1.3

73.5 ± 1.6

54.6 ± 3.4

7

-

-

65.8 ± 2.4

67.7 ± 1.4

52.0 ± 3.9

14

-

-

68.0 ± 1.0

68.2 ± 2.9

50.0 ± 2.8

21

-

-

65.9 ± 1.7

66.5 ± 1.4

49.7 ± 3.7