Figure 5From: Hydrothermal treatment of Ti surface to enhance the formation of low crystalline hydroxyl carbonate apatite Concentrations of remained Ca and P ions in SBF after 1, 3 and 7 day immersion of various types of titanium samples; machined, and blasted, alkali etched, blasted-etched. Back to article page